1.交货条款组合
表C.1 -交货时热处理条件、产品形式和适用要求的组合
| Heat-treatment condition at delivery | Symbo | Products form a | Applicable requirements in cases where the steel concerned has been ordered with reference to the steel names indicated in | ||||||||||
| Wire rod | Bar | Wire | Tables C.2,C.3,C.4, C.5 or C.6 | Tables C.2,C.3,C.4,C.5,C,6,C.Z C.8 or C.9 | Tables C.2,C.3,C.4,C.5,C.6 or C.10 | Optional | |||||||
| As hot-rolled or peeled | +AR or +PE | X | X | X | Chemical compo- sition as speci- fied in Tables C.2 and C.3 | Me- chanical properties as spec- ified in Tables C.4. C.5 and C.6 | Chemical compo- sition as speci- fied in Tables C.2 and C.3 | Me- chanical properties as spec- ified in Tables C.4, C.5 and C.6 | Values for harden- ability according to Tables C.Z C.8 and C.9 | Chemical compo- sition as speci- fied in Tables C.2 and C.3 | Me- chanical properties as spec- ified in Tables C.4. C.5 and C.6 | Mini- mum core hardness and max- imum diameter accord- ing to TableC.10 | Supplementa- ry or special requirements as specified in Annex Eb |
| Cold drawn | +AR +C | — | X | X | |||||||||
| Cold drawn + spheroidized | +AR+C+ AC | — | X | X | |||||||||
| Cold drawn + spheroidized + skin passed | +AR+C +AC +LC | — | X | X | |||||||||
| Spheroidized or spheroidized + peeled | +AC or +AC+PE | X | X | X | |||||||||
| Spheroidized + cold drawn | +AC+C | — | X | X | |||||||||
| Spheroidized+ cold drawn +spheroidized | +AC+C+ AC | X | X | ||||||||||
| Spheroidized + cold drawn +sphe- roidized +skin passed | +AC+C+ AC+LC | X | X | ||||||||||
| Others | Other delivery conditions may be agreed at the time of ordering | ||||||||||||
| a X=applicable,—=not applicable b If agreed at the time of the enquiry and order. | |||||||||||||
2.化学成分
表C.3-调质用含氮合金钢牌号的化学成分(适用于铸造分析)
| Steel name b | % mass fraction | ||||||||||||
| C | Si c | Mn | P | S | Cr d | Mo | B | Cu | |||||
| 17B2 | 0,15 to 0,20 | 0,30 | 0,60 to 0,90 | 0,025 | 0,025 | 0,30 | 0,0008 to 0,005 | 0,25 | |||||
| 23B2 | 0,20 to 0,25 | 0,30 | 0,60 to 0,90 | 0,025 | 0,025 | 0,30 | 0,0008 to 0,005 | 0,25 | |||||
| 28B2 | 0,25 to 0,30 | 0,30 | 0,60 to 0,90 | 0,025 | 0,025 | 0,30 | —— | 0,0008 to 0,005 | 0,25 | ||||
| 33B2 | 0,30 to 0,35 | 0,30 | 0,60 to 0,90 | 0,025 | 0,025 | 0,30 | — | 0,0008 to 0,005 | 0,25 | ||||
| 38B2 | 0,35 to 0,40 | 0,30 | 0,60 to 0,90 | 0,025 | 0,025 | 0,30 | — | 0,0008 to 0,005 | 0,25 | ||||
| 23MnB3 | 0,21 to 0,25 | 0,15 | 0,80 to 1,00 | 0,015 | 0,015 | 0,25 to 0,35 | — | 0,0008 to 0,005 | 0,25 | ||||
| 17MnB4 | 0,15 to 0,20 | 0,30 | 0,90 to 1,20 | 0,025 | 0,025 | 0,30 | — | 0,0008 to 0,005 | 0,25 | ||||
| 20MnB4 | 0,18 to 0,23 | 0,30 | 0,90 to 1,20 | 0,025 | 0,025 | 0,30 | 0,0008 to 0,005 | 0,25 | |||||
| 23MnB4 | 0,20 to 0,25 | 0,30 | 0,90 to 1,20 | 0.025 | 0,025 | 0,30 | — | 0,0008 to 0,005 | 0,25 | ||||
| 27MnB4 | 0,25 to 0,30 | 0,30 | 0,90 to 1,20 | 0,025 | 0,025 | 0,30 | — | 0,0008 to 0,005 | 0,25 | ||||
| 30MnB4 | 0,27 to 0,32 | 0,30 | 0,80 to 1,10 | 0,025 | 0,025 | 0,30 | — | 0,0008 to 0,005 | 0,25 | ||||
| 36MnB4 | 0,33 to 0,38 | 0,30 | 0,80 to 1,10 | 0,025 | 0,025 | 0,30 | — | 0,0008 to 0,005 | 0,25 | ||||
| 20MnB5 | 0,17 to 0,23 | 0,30 | 1,10 to 1,40 | 0,025 | 0,025 | 0,30 | — | 0,0008 to 0,005 | 0,25 | ||||
| 23MnB5 | 0,20 to 0,26 | 0,30 | 1,10 to 1,40 | 0,025 | 0,025 | 0,30 | — | 0,0008 to 0,005 | 0,25 | ||||
| 26MnB5 | 0,23 to 0,29 | 0,30 | 1,20 to 1,50 | 0,025 | 0,025 | 0,30 | — | 0,0008 to 0,005 | 0,25 | ||||
| 34MnB5 | 0,31 to 0,37 | 0,30 | 1,20 to 1,50 | 0,025 | 0,025 | 0,30 | — | 0,0008 to 0,005 | 0,25 | ||||
| 37MnB5 | 0,35 to 0,40 | 0,30 | 1,15 to 1,45 | 0,025 | 0,025 | 0,30 | — | 0,0008 to 0,005 | 0,25 | ||||
| 30MoB1 | 0,28 to 0,32 | 0,30 | 0,80 to 1,00 | 0,025 | 0,025 | 0,30e | 0,08 to 0,12 | 0,0008 to 0,005 | 0,25 | ||||
| |||||||||||||
3.力学性能
表C.6 -含氮合金钢牌号的机械性能
| Steel name | Diameter | Delivery condition | ||||||||||||
| +AR or +PE | +AC or +AC+PE | +AR+C | +AR+C+AC | +AR+C+AC+LC | +AC+C | |||||||||
| Mechanical properties | ||||||||||||||
| above mm | up to mm | Rm max. MPa | Z min. % | Rm max. MPa | Z min. % | Rm max MPa | Z min. % | Rm max. MPa | Z min. % | Rm max. MPa | Z min. % | Rm max. MPa | Z min. % | |
| 20MnB4 | 2 | 5 | — | 490 | 68 | 530 | 66 | — | ||||||
| 5 | 10 | 580 | 60 | 500 | 66 | 680 | 55 | 480 | 68 | 520 | 66 | 600 | 61 | |
| 10 | 25 | 580 | 60 | 500 | 66 | 670 | 55 | 480 | 68 | 520 | 66 | 590 | 61 | |
| 23MnB4 | 2 | 5 | 510 | 66 | 550 | 64 | — | |||||||
| 5 | 10 | 600 | 60 | 520 | 64 | 700 | 55 | 500 | 66 | 540 | 64 | 620 | 59 | |
| 10 | 25 | 600 | 60 | 520 | 64 | 690 | 55 | 500 | 66 | 540 | 64 | 610 | 59 | |
| 27MnB4 | 2 | 5 | — | — | 530 | 65 | 570 | 63 | ||||||
| 5 | 40 | — | 540 | 63 | — | 520 | 65 | 560 | 63 | 640 | 58 | |||
| 30MnB4 | 2 | 5 | 一 | — | — | 560 | 65 | 600 | 63 | — | — | |||
| 5 | 40 | —— | — | 570 | 63 | — | 550 | 65 | 590 | 63 | 670 | 58 | ||
| 36MnB4 | 2 | 5 | — | —— | 一 | — | —— | 590 | 64 | 630 | 62 | — | ||
| 5 | 40 | — | — | 600 | 62 | — | — | 580 | 64 | 620 | 62 | 700 | 57 | |
| 20MnB5 | 2 | 5 | — | 630 | 55 | — | ||||||||
| 5 | 40 | — | 一 | — | — | — | 630 | 55 | 630 | 55 | ||||
| 23MnB5 | 2 | 5 | — | — | — | — | — | — | — | — | 640 | 55 | — | |
| 5 | 40 | — | — | — | — | — | — | 640 | 55 | 640 | 55 | |||
| 26MnB5 | 2 | 5 | — | 一 | — | — | 一 | 650 | 55 | — | — | |||
| 5 | 40 | — | — | — | — | 650 | 55 | 650 | 55 | |||||
| 34MnB5 | 2 | 5 | — | — | — | — | — | — | — | 680 | 55 | — | — | |
| 5 | 40 | — | — | 一 | 一 | — | 一 | 680 | 55 | 680 | 55 | |||
| 37MnB5 | 2 | 5 | — | 610 | 64 | 650 | 62 | — | ||||||
| 5 | 40 | — | 620 | 62 | — | — | 600 | 64 | 640 | 62 | 720 | 57 | ||
| It should be recognized in the +AR condition that the tensile strength values are not compatible with the whole range of composition given in TableC.3 for a steel grade.Care should be taken that,depending on diameter and composition supplied,the tensile strength values are compatible with the hardenability requirements. | ||||||||||||||
4.硬化性要求
表C.8 -具有标准硬化性(+H级)的含氮合金钢牌号的硬度极限