上海睿雄实业集团是中国.是一家有20年经验的基准企业,在所有管理层都专注于冷镦用优质钢丝。我们与汽车产业的很多tia1供应商建立了良好的关系,所有的线材都是由品牌的钢铁厂提供的。所有订单均可100% 跟踪。
COLD FORMING MATERIALS
S33C冷镦用钢丝
MATERIALSENGINEERINGCREATION GROUP
CREATION GROUP / ZH

1.化学成分
表2-化学成分,单位 %
| 牌号 | C | Si | Mn | P | S | Ni | Cr a) | Cu | Ni+Cr b) |
| S10C | 0.08~0.13 | 0.15~0.35 | 0.30~0.60 | ≤0.030 | ≤0.035 | ≤0.20 | ≤0.20 | ≤0.30 | ≤0.35 |
| S12C | 0.10~0.15 | 0.15~0.35 | 0.30~0.60 | ≤0.030 | ≤0.035 | ≤0.20 | ≤0.20 | ≤0.30 | ≤0.35 |
| S15C | 0.13~0.18 | 0.15~0.35 | 0.30~0.60 | ≤0.030 | ≤0.035 | ≤0.20 | ≤0.20 | ≤0.30 | ≤0.35 |
| S17C | 0.15~0.20 | 0.15~0.35 | 0.30~0.60 | ≤0.030 | ≤0.035 | ≤0.20 | ≤0.20 | ≤0.30 | ≤0.35 |
| S20C | 0.18~0.23 | 0.15~0.35 | 0.30~0.60 | ≤0.030 | ≤0.035 | ≤0.20 | ≤0.20 | ≤0.30 | ≤0.35 |
| S22C | 0.20~0.25 | 0.15~0.35 | 0.30~0.60 | ≤0.030 | ≤0.035 | ≤0.20 | ≤0.20 | ≤0.30 | ≤0.35 |
| S25C | 0.22~0.28 | 0.15~0.35 | 0.30~0.60 | ≤0.030 | ≤0.035 | ≤0.20 | ≤0.20 | ≤0.30 | ≤0.35 |
| S28C | 0.25~0.31 | 0.15~0.35 | 0.60~0.90 | ≤0.030 | ≤0.035 | ≤0.20 | ≤0.20 | ≤0.30 | ≤0.35 |
| S30C | 0.27~0.33 | 0.15~0.35 | 0.60~0.90 | ≤0.030 | ≤0.035 | ≤0.20 | ≤0.20 | ≤0.30 | ≤0.35 |
| S33C | 0.30~0.36 | 0.15~0.35 | 0.60~0.90 | ≤0.030 | ≤0.035 | ≤0.20 | ≤0.20 | ≤0.30 | ≤0.35 |
| S35C | 0.32~0.38 | 0.15~0.35 | 0.60~0.90 | ≤0.030 | ≤0.035 | ≤0.20 | ≤0.20 | ≤0.30 | ≤0.35 |
| S38C | 0.35~0.41 | 0.15~0.35 | 0.60~0.90 | ≤0.030 | ≤0.035 | ≤0.20 | ≤0.20 | ≤0.30 | ≤0.35 |
| S40C | 0.37~0.43 | 0.15~0.35 | 0.60~0.90 | ≤0.030 | ≤0.035 | ≤0.20 | ≤0.20 | ≤0.30 | ≤0.35 |
| S43C | 0.40~0.46 | 0.15~0.35 | 0.60~0.90 | ≤0.030 | ≤0.035 | ≤0.20 | ≤0.20 | ≤0.30 | ≤0.35 |
| S45C | 0.42~0.48 | 0.15~0.35 | 0.60~0.90 | ≤0.030 | ≤0.035 | ≤0.20 | ≤0.20 | ≤0.30 | ≤0.35 |
| S48C | 0.45~0.51 | 0.15~0.35 | 0.60~0.90 | ≤0.030 | ≤0.035 | ≤0.20 | ≤0.20 | ≤0.30 | ≤0.35 |
| S50C | 0.47~0.53 | 0.15~0.35 | 0.60~0.90 | ≤0.030 | ≤0.035 | ≤0.20 | ≤0.20 | ≤0.30 | ≤0.35 |
| S53C | 0.50~0.56 | 0.15~0.35 | 0.60~0.90 | ≤0.030 | ≤0.035 | ≤0.20 | ≤0.20 | ≤0.30 | ≤0.35 |
| S55C | 0.52~0.58 | 0.15~0.35 | 0.60~0.90 | ≤0.030 | ≤0.035 | ≤0.20 | ≤0.20 | ≤0.30 | ≤0.35 |
| S58C | 0.55~0.61 | 0.15~0.35 | 0.60~0.90 | ≤0.030 | ≤0.035 | ≤0.20 | ≤0.20 | ≤0.30 | ≤0.35 |
| S09CK | 0.07~0.12 | 0.10~0.35 | 0.30~0.60 | ≤0.025 | ≤0.025 | ≤0.20 | ≤0.20 | ≤0.25 | ≤0.30 |
| S15CK | 0.13~0.18 | 0.15~0.35 | 0.30~0.60 | ≤0.025 | ≤0.025 | ≤0.20 | ≤0.20 | ≤0.25 | ≤0.30 |
| S20CK | 0.18~0.23 | 0.15~0.35 | 0.30~0.60 | ≤0.025 | ≤0.025 | ≤0.20 | ≤0.20 | ≤0.25 | ≤0.30 |
本表中未规定的元素,除了完成钢水的目的以外,不得有意添加。
注a) 根据交接当事人之间的协定可以小于0.30%。
b) 根据交接当事人间的协定,Ni + Cr的上限为,S09CK、S15CK及S20CK不足0.40%,其他种类为,也可以小于0.45%。
注a) 根据交接当事人之间的协定可以小于0.30%。
b) 根据交接当事人间的协定,Ni + Cr的上限为,S09CK、S15CK及S20CK不足0.40%,其他种类为,也可以小于0.45%。
2.线材的力学性能
在交接当事人之间,有时会协定机械性质的值。
3.尺寸公差
表8-热轧线的尺寸公差
| 直径 | 直径公差 | 偏径差 a) |
| <15 | ±0.3 | <0.4 |
| 15<d≤25 | ±0.4 | <0.5 |
| 25<d≤32 | ±0.5 | <0.6 |
| 32<d≤50 | ±0.6 | <0.7 |
直径超过50mm的线材尺寸的容许差,取决于交接当事人之间的协定。
注a) 偏径差是指线材在同一截面中的直径的最大值与最小值之差。
注a) 偏径差是指线材在同一截面中的直径的最大值与最小值之差。
1、 成卷
线材捆扎示例
2、 长条状
线材捆扎示例
3、 外销木箱包装
线材捆扎示例
4、 装柜照片
装柜照片
5、 产品防护细节
产品防护
5、 产品防护细节
产品防护
外包装示例
端面木板包装
缠绕包装
PP布袋套袋包装
线架包装