COLD FORMING MATERIALS
SAE4042 AISI4042 ASTM4042 冷镦用钢丝(CHQ)
MATERIALSENGINEERINGCREATION GROUP
CREATION GROUP / ZH

SAE4042 AISI4042 ASTM4042 冷镦用钢丝(CHQ)
1.提供的条件和化学组成
表7合金钢的化学范围和限值,%
| IFI Steel Grade Designation | Carbon | Manganese | Nickel | Chromium | Molybdenum | Phosphorous | Sulfur | |||||
| Min | Max | Min | Max | Min | Max | Min | Max | Min | Max | Max | Max | |
| IFI-1335 | 0.33 | 0.38 | 1.60 | 1.90 | ... | ... | ... | ... | ... | ... | 0.020 | 0.020 |
| IFI-4037A | 0.35 | 0.40 | 0.70 | 0.90 | ... | ... | ... | ... | 0.20 | 0.30 | 0.020 | 0.020 |
| IFI-4042 | 0.40 | 0.45 | 0.70 | 0.90 | ... | ... | ... | ... | 0.20 | 0.30 | 0.020 | 0.020 |
| IFI-4118 | 0.18 | 0.23 | 0.70 | 0.90 | ... | ... | 0.40 | 0.60 | 0.08 | 0.15 | 0.020 | 0.020 |
| IFI-4140 | 0.38 | 0.43 | 0.75 | 1.00 | ... | ... | 0.80 | 1.10 | 0.15 | 0.25 | 0.020 | 0.020 |
| IFI-5140 | 0.38 | 0.43 | 0.70 | 0.90 | ... | ... | 0.70 | 0.90 | ... | ... | 0.020 | 0.020 |
| IFI-8637 | 0.35 | 0.40 | 0.75 | 1.00 | 0.40 | 0.70 | 0.40 | 0.60 | 0.15 | 0.25 | 0.020 | 0.020 |
A在Alk或siFg或sicg或cgp中提供。siFg中的所有其他等级-仅限Fg。
表8规定化学范围和AIIoy SteeIs限值的允许偏差,%
| Element | Limit or Max of specified Range, % | variation, %, overMax Limit orunder Min Limit |
| Carbon | To 0.30 inclover 0.30 to 0.75 incl | 0.01 |
| 0.02 | ||
| Manganese | To 0.90 inclover 0.90 | 0.03 |
| 0.04 | ||
| phosphorus | over Max only | 0.005 |
| Sulfur | over Max only | 0.005 |
| Silicon | To 0.40 incl | 0.02 |
| Nickel | To 1.00 incl | 0.03 |
| Chromium | To 0.90 inclover 0.90 | 0.03 |
| 0.05 | ||
| Molybdenum | To 0.20 inclover 0.20 to 0.40 incl | 0.01 |
| 0.02 | ||
| vanadium | over Max only | 0.01 |
| copper | over Max only | 0.03 |
2.力学性能
表11碳钢和合金钢力学性能
| Steel Grade | Rod/Bar properties | Spheroidize Annealed at Finished Size wire properties | Annealed in process andSpheroidized Annealed in processFinished wire properties | |||||||
| Annealed | Spheroidize Annealed | SAFS | AIP | SAIP | ||||||
| Max tensileA | MinR/A | Max tensileA | MinR/A | Max tensileA | MinR/A | Max tensileA | MinR/A | Max tensileA | MinR/A | |
| KSI | % | KSI | % | KSI | % | KSI | % | KSI | % | |
| Carbon | ||||||||||
| IFI-1006 | 55 | 62 | 53 | 65 | 51 | 70 | 62 | 60 | 60 | 62 |
| IFI-1008 | 56 | 62 | 54 | 65 | 52 | 70 | 63 | 60 | 61 | 62 |
| IFI-1010 | 58 | 62 | 55 | 65 | 54 | 70 | 65 | 60 | 62 | 62 |
| IFI-1018 | 68 | 62 | 65 | 65 | 63 | 68 | 76 | 60 | 68 | 62 |
| IFI-1022/A | 72 | 62 | 67 | 65 | 65 | 68 | 81 | 60 | 72 | 62 |
| IFI-1022/B | 73 | 62 | 69 | 65 | 67 | 68 | 82 | 60 | 73 | 62 |
| IFI-1033 | 80 | 58 | 74 | 60 | 72 | 64 | 89 | 56 | 82 | 58 |
| IFI-1035 | 81 | 58 | 75 | 60 | 73 | 64 | 90 | 56 | 83 | 58 |
| IFI-1038 | 82 | 58 | 76 | 60 | 74 | 64 | 91 | 56 | 84 | 58 |
| IFI-1541A | 92 | 53 | 85 | 57 | 82 | 61 | 98 | 51 | 92 | 55 |
| IFI-1541B | 93 | 53 | 86 | 57 | 83 | 61 | 99 | 51 | 93 | 55 |
| Boron | ||||||||||
| IFI-10B21 | 75 | 62 | 71 | 64 | 69 | 68 | 84 | 60 | 75 | 62 |
| IFI-10B38 | 88 | 56 | 82 | 58 | 80 | 62 | 97 | 52 | 90 | 56 |
| Alloy | ||||||||||
| IFI-1335 | 93 | 53 | 85 | 55 | 82 | 59 | 100 | 51 | 92 | 53 |
| IFI-4037 | 86 | 55 | 80 | 57 | 78 | 60 | 95 | 53 | 85 | 55 |
| IFI-4042 | 88 | 55 | 82 | 57 | 80 | 60 | 97 | 53 | 87 | 55 |
| IFI-4118 | 76 | 60 | 71 | 61 | 68 | 64 | 84 | 58 | 76 | 59 |
| IFI-4140 | 92 | 55 | 85 | 57 | 82 | 59 | 102 | 53 | 90 | 55 |
| IFI-5140 | 92 | 55 | 85 | 57 | 82 | 59 | 102 | 53 | 90 | 55 |
| IFI-8637 | 92 | 53 | 85 | 55 | 82 | 57 | 102 | 51 | 92 | 53 |
A对于铝镇静钢,减去3 KSI并增加1% R/A。
对于沸腾钢,减去5 KSI并增加2% R/A。
对于0.200英寸以下的AIp和SAIP钢丝,每0.001英寸增加50 psi。在0.200之下。
注1-本表中的值旨在在冷成型过程中提供最佳的冷镦成形性和模具寿命。断面收缩率试验不适用于钢丝尺寸小于0.092 in.
对于沸腾钢,减去5 KSI并增加2% R/A。
对于0.200英寸以下的AIp和SAIP钢丝,每0.001英寸增加50 psi。在0.200之下。
注1-本表中的值旨在在冷成型过程中提供最佳的冷镦成形性和模具寿命。断面收缩率试验不适用于钢丝尺寸小于0.092 in.
3.脱碳限值
表10碳含量超过0.15% 的烧钢的脱碳限值
| Diameter,in. | Free Ferrite Depthmax, in. | Total Average Affected Depth(TAAD) max, in. | worst Location Depth,max, in. |
| through 25/64 | 0.001 | 0.005 | 0.008 |
| over 25/64through 5/8 | 0.001 | 0.006 | 0.009 |
| over 5/8through 55/64 | 0.001 | 0.007 | 0.011 |
| over 55/64through 1 | 0.001 | 0.008 | 0.012 |
| over 1through 1-1/2 | 0.001 | 0.010 | 0.015 |